Schlauch White
APPLICATION
Flexo printing
External printing
PROPOSED MATERIALS
Corona treated PE > 38 dyne/cm
Corona treated OPP and Coex > 38 dyne/cm
Corona treated cast OPP > 38 dyne/cm
Chemically treated PET
Corona treated OPA > 48 dyne/cm
NC primed aluminum foil
All types of paper
CHARACTERISTICS
Good adhesion
Good mechanical resistance
Good intensity
High gloss
Resistance to high temperatures:
Up to 180 °C, tested at LDPE
Up to 140 °C, tested at OPP, Coex
Duraflex White
APPLICATION
Flexo printing
Internal printing
PROPOSED MATERIALS
Corona treated PE > 38 dyne/cm
Corona treated PET > 48 dyne/cm
Chemically treated PET > 48 dyne/cm
Corona treated OPP > 38 dyne/cm
Corona treated PA > 48 dyne/cm
CHARACTERISTICS
Suitable for pasteurization at approx. 100 °C
Suitable for lamination on a wide range of materials
Good intensity
Duraline V AP2 White
APPLICATION
Flexo printing
External and internal printing
PROPOSED MATERIALS
Corona treated PE > 38 dyne/cm
Corona treated OPP and Coex > 38 dyne/cm
Chemically treated PET
NC primed aluminum foil
All types of paper
CHARACTERISTICS
Good adhesion
Good mechanical resistance
Good intensity
High gloss
Resistance to high temperatures, 170 °C
Solimax P AP White HC
APPLICATION
Flexo printing
External and internal printing
PROPOSED MATERIALS
Corona treated PE > 38 dyne/cm
Corona treated OPP, OT and Coex > 38 dyne/cm
Corona treated cast OPP > 38 dyne/cm
Corona treated PET > 48 dyne/cm
Chemically treated PET
Corona treated OPA > 48 dyne/cm
Chemically treated OPA
NC primed aluminum foil
All types of paper
CHARACTERISTICS
Good adhesion
Good mechanical resistance
High pigmentation and colour coverage
High gloss
Resistance to high temperatures, 180-200 °C
Solvaplast T White
APPLICATION
Flexo printing
External printing
PROPOSED MATERIALS
Corona treated PE > 38 dyne/cm
Corona treated OPP and Coex > 38 dyne/cm with addition of 4-5% adhesive promoter
Corona treated cast OPP > 38 dyne/cm
NC primed aluminum foil
All types of paper
CHARACTERISTICS
Good adhesion
Good mechanical resistance
Good intensity
High gloss
Resistance to high temperatures:
Up to 160 °C for PE, without the adhesive promoter
Up to 180-200 °C for PP, with addition of 4-5% adhesive promoter